Rauschert Ceramic infra-red plaque 26515/1-8101-101
SKU 26515/1-8101-101
Brand Rauschert
Photos
Key specifications
| Length | 132 mm |
|---|---|
| Width | 92 mm |
| Height | 13 mm |
| material | technical ceramics |
| Function | Produces even high-temperature infrared radiation |
| Chemical resistance | increased resistance to chemical exposure |
| Catalogue article numbers | 26515/1-8101-101, 804.579.005 |
| Thermal resistance | withstands repeated thermal cycling |
| Dielectric properties | excellent |
| Dimensional stability | stable |
| Mechanical resistance | resistant to mechanical loads |
| Porosity | porous |
23.96 EUR
21.78EUR
in stock · 5
incl. 21% VAT · 18.00 EUR excl. VAT · shipping calculated at checkout
- Worldwide shipping from stock
- Original manufacturer part
- Dispatch within 24 h for stocked items
Description
This ceramic infra-red plaque (132 mm × 92 mm × 13 mm) is made of porous technical ceramics. It is installed in gas burners using radiant surface combustion, where the gas-air mixture burns across the plaque surface to produce even high-temperature infrared radiation. The material withstands repeated thermal cycling, resists chemical exposure, and maintains stable dimensions under mechanical load. Its porous structure keeps the mixture permeable, while its dielectric and mechanical properties suit demanding burner applications.
Further details
| Application | Gas burners that use radiant surface combustion |
|---|
Choosing and fitting
Plaques of this type are selected by overall dimensions (length, width, thickness) and the shape of the mounting edges, as the part sits in a metal frame or is held by a sealing gasket. Before fitting, inspect the burner frame distortion and gasket condition; an uneven seal causes local overheating and early failure. Verify gas pressure and air adjustment within the manufacturer's range for infra-red operation — improper mixture leads to sooting or overheating. When a burner uses multiple plaques, replace the full set to ensure uniform radiation and avoid thermal stress from mismatched ageing.
Signs of failure
Visible defects such as cracks, chips, or glaze separation cause flashback or incomplete combustion. Local overheating appears when the seal against the frame is uneven, often leading to early failure. Sooting or overheating of the plaque indicates incorrect gas/air mixture. Check the plaque surface for burnout patterns and inspect the frame and gasket for damage.
All specifications
| Length | 132 mm |
|---|---|
| Width | 92 mm |
| Height | 13 mm |
| material | technical ceramics |
| Function | Produces even high-temperature infrared radiation |
| Chemical resistance | increased resistance to chemical exposure |
| Catalogue article numbers | 26515/1-8101-101, 804.579.005 |
| Thermal resistance | withstands repeated thermal cycling |
| Dielectric properties | excellent |
| Dimensional stability | stable |
| Mechanical resistance | resistant to mechanical loads |
| Porosity | porous |
Part numbers
| SKU | 26515/1-8101-101 |
|---|---|
| Additional article | 804.579.005 |